Stripping and galvanizing lines
Topic
The stripping and galvanizing lines protect cold rolled steel against corrosion. Stripping removes the oxide husk formed during hot rolling by hydrochloric acid or sulfuric acid baths; Galvanizing applies a layer of zinc cast by immersion (Hot-dip galvanizing) or electrochemically. The physical model integrates acid corrosion kinetics, zinc mass transfer and mechanics of the strip. Iron oxide pickling (mainly ugly, Fe3O4 and Fe2O3) in HCl follows the Arrhenius kinetics: the rate of dissolution is proportional to the concentration of acid and grows exponentially with temperature; Modern lines operate at 70-90 C to maximize speed without attacking base steel. In hot dip galvanization, the flux-coated, cleaned steel strip enters a fused zinc bath at 450-490 C; Zinc forms a Fe-Zn alloy layer at the interface (gamma, delta, zeta phases) and a pure zinc layer on the outer surface. The flow of zinc to the substrate follows Fick's law for the diffusion film in the liquid bath. The thickness of the deposited layer depends on the immersion time and the zinc flow; The typical weights are 275-600 g/m^2 (both faces). At the exit of the bathroom, the air knives control the thickness of zinc by the force of the high-speed jet on the liquid zinc layer that drains from the strip: the force of the jet follows the mechanics of impact fluids. The steel strip must be kept under controlled tension along the entire line to prevent deformation and guarantee the quality of the coating; The tension force follows the material resistance formula. The expected behavior is that the zinc weight is inversely proportional to the speed of the strip (lower speed, greater immersion time and greater weight) and directly proportional to the pressure of the air knife (higher pressure blows more zinc from the strip).
ID:5230