BOF Converters (Basic Oxygen Furnace)
Topic
The BOF converter fine-tunes the blast furnace liquid iron by high-speed injection of pure oxygen from a spear over the metal bath. The process takes 15-25 minutes and removes excess carbon, silicon, manganese and cast iron phosphorus. The physical model integrates kinetic decarburation, energy balance and metallurgical thermodynamics of slag-metal reactions. Decarburation follows a pseudo-first order kinetics with respect to oxygen flow and carbon content: at high carbon contents, the velocity is proportional to the oxygen flow rate (O2-controlled stage); Below 0.1% carbon the speed is controlled by mass transfer of coal into the bathroom. The total oxygen required results from the stoichiometry of the oxidation of carbon to CO/CO2. The process is strongly exothermic: the oxidation of each kilogram of carbon generates 33 MJ of heat, so the bath temperature rises from the 1350 C of the cast iron to 1600-1700 C of the tuned steel No external energy input. The lance oxygen jet is supersonic (Mach 2-3) at the outlet of the convergent-divergent nozzle; The dynamic pressure of the jet creates a crater in the bathroom that favors mixing and reaction. The distribution of sulfur between slag and metal follows Richardson's thermodynamic equilibrium: the greater the basicity of slag (higher CaO activity) and lower ugly content, higher sulfur transfer to metal to slag. The blow time is the ratio between the total oxygen required and the flow rate of the lance. The expected behavior is that the bath temperature must reach the casting temperature (1600-1700 C) at the end of the murmur simultaneously with the target carbon content; The temperature and the carbon are the two control variables of the end of the blow.
ID:5226